Home> PHENOLIC REINFORCING RESIN

PHENOLIC REINFORCING RESINS

Phenolic resins are modified with cashew nut shell liquid, or tall oil, or are unmodified phenol formaldehyde resin. They are premixed with hexamine as a curing agent. Incorporation of these resins in rubber compounds enhances resistance towards heat, water, oil, hydrocarbons, etc., while improving mechanical properties such as tensile strength, tear strength, and abrasion resistance.

Resin Type
Typical Properties
PP-1711
Modified phenol formaldehyde resin with HMT
Melting Point (°C): 65 - 90
Hexa Content (%): 9 - 11
PP-1720
Modified phenol formaldehyde resin with HMT
Melting Point (°C): 70 - 85
Hexa Content (%): 10 - 12
PP-1811
Modified phenol formaldehyde resin with HMT
Melting Point (°C): 70 - 80
Hexa Content (%): 6 - 9
Modified phenol formaldehyde resin with HMT
Melting Point (°C): 65 - 90
Hexa Content (%): 5-7
PP-1913
Modified phenol formaldehyde resin with HMT
Melting Point (°C): 70 - 85
Hexa Content (%): 9 - 11
PP-1817
Modified phenol formaldehyde resin with HMT
Melting Point (°C): 72 - 85
Hexa Content (%): 6.5 - 8.5
PP-1819
Phenol formaldehyde resin premixed with HMT
Melting Point (°C): 80 - 100
Hexa Content (%): 8-10
PP-1910
Phenol formaldehyde resin premixed with HMT
Melting Point (°C): 80 - 100
Hexa Content (%): 6.5 - 8.5

PHENOLIC REINFORCING NOVALAK RESIN

Phenolic novalak resins are modified with cashew nut shell liquid, or tall oil, or are unmodified phenol formaldehyde resin with very low residual free phenol levels. Novalak resins require the addition of hexamine to make them thermosetting. These are designed for high temperature compounding cycles where the early presence of hexamine could result in scorching.

Resin Type
Typical Properties
PP-1811N
Cashew modified phenol formaldehyde resin
Softening Point (°C): 90 - 100
Free Phenol (%): < 1.0
PP-1817N
Tall oil modified phenol formaldehyde resin
Softening Point (°C): 90 - 105
Free Phenol (%): < 1.0
Ash Content (%): < 0.50
PP-1818
Phenol formaldehyde resin
Softening Point (°C): 104 - 116
Free Phenol (%): < 1.0
Ash Content (%): < 0.10
Phenol formaldehyde resin
Softening Point (°C): 80 - 100
Free Phenol (%): < 0.50
Ash Content (%): < 0.50
PP-1818M
Phenol formaldehyde resin
Softening Point (°C): 98 - 110
Free Phenol (%): < 0.50
Ash Content (%): < 0.10
PP-2160
Alkyl modified phenol-formaldehyde reinforcing resin
Softening Point (°C): 101 - 113
Free Phenol (%): < 1.0
Ash Content (%): < 0.10
Singh Plasticisers and Resins (India) Private Limited
Why Choose Our PHENOLIC REINFORCING RESIN?

Commitment to Excellence

Quality drives everything we do. Our PHENOLIC REINFORCING RESINS undergo rigorous testing to ensure consistent performance, reliability, and excellence in rubber manufacturing.

Tailored Expertise

Partner with us for personalized support. POWERPLAST offers dedicated expertise and customized solutions to ensure the success of your projects with our PHENOLIC REINFORCING RESINS

Sustainable Innovation

Sustainability meets performance with our PHENOLIC REINFORCING RESINS. Crafted with eco-conscious materials, they provide environmentally friendly solutions without compromising quality, helping to create a greener future.

Exceptional Phenolic Performance

Our PHENOLIC REINFORCING RESINS strengthen the bond between rubber and reinforcements, delivering durable, long-lasting connections for reliable rubber products.

Safety-Centric Solutions

POWERPLAST PHENOLIC REINFORCING RESINS are designed with safety in mind, offering lower toxicity compared to traditional alternatives, ensuring the well-being of your team and reducing environmental impact.

Enhanced Versatility

Achieve superior performance with our PHENOLIC REINFORCING RESINS, which optimize key properties like modulus, tensile strength, stiffness, and hardness, ensuring exceptional results in rubber applications.

With 40+ years of experience, SPR is your trusted partner for innovative chemical solutions. Specializing in POWERPLAST Rubber Processing Chemicals and Dry Bonding Agents. Choose SPR for unparalleled excellence.

Contact Info

Copyright © 2025 Power-Plast Developed by DebateMarketers